NONWOVEN
General properties of "TERRAMAC" spunbonds
Unit | G0203WTO | G0303WTO | G0403WTO | G0503WTO | G0703WTO | G1003WTO | ||
Weight | g/m² | 20 | 30 | 40 | 50 | 70 | 100 | |
Thickness | µm | 140 | 210 | 240 | 300 | 400 | 510 | |
Tensile strength |
MD | N/5cm | 45 | 65 | 70 | 90 | 120 | 175 |
TD | 20 | 30 | 35 | 40 | 85 | 120 | ||
Tensile elongation |
MD | % | 15 | 15 | 15 | 17 | 17 | 20 |
TD | 15 | 15 | 15 | 17 | 17 | 18 | ||
Tearing strength |
MD | N | 3 | 4 | 5 | 5 | 5 | 6 |
* The data above are typical values of test pieces measured by methods compliant with JIS L-1906,
and are not intended to guarantee the properties of resins in a particular application.